No 名称 Name No 名称 Name
51 形状 Shape 5101 无夹砂的外膨胀 Swelling outside extra without sand inclusions (soft spot mould)
5102 无夹砂的内膨胀 Swelling inside extra without sand inclusions (soft spot core and or mould)
5103 凸出或者凹陷  Strain (swelling + thick fins or flash) or Sag
5104 紧实错型导致的多肉 Ramoff, Ramaway
5105 拔砂&类似拔砂造成的多肉 Sticker (sand removed with pattern) & sticker like
5106 砂芯破裂造成的多肉 Broken or crushed core
5107 缺少砂芯造成的多肉 Material due to lacking core
52 形状&夹砂  Shape & sand inclusions 5201 砂芯/芯冲蚀 Erosion – mould/core wash / with or without small sand inclusion; Ingate area     
5202 其他区域的砂型磨损 Sand abrasion other area
5203 型砂破碎(掉进去) Broken sand (Drop)
5204 型砂破碎(冒口底部) Broken sand (Bottom rise)
5205 型砂破碎(铸型挤压) Broken sand (Mould crush)
5206 内腔形状(砂芯损坏) Inside shape (broken core)
5207 铸件内腔和外观多肉 In- and outside extra metal
53 焊层 Weld layer 5301 多余 Weld layer
5302 区部没有清理的多余焊接材料 Weld remains locally
54 披缝 Flash 5401 铸型分型面处的披缝 Mould split line
5402 外表面-铸型破裂处的披缝  Outside surface – Cracked mould…
5403 分芯面处的披缝 Core split line
5404 内表面的披缝 Inside surface
5405 铸型-砂芯连接处披缝  Mould-core connection
5406 砂芯-砂芯连接处披缝  Core-core connection
5407 分型面&型-芯连接处的披缝  Split line & mould-core connection
55 特殊的细微结构 Special details 5501 激冷筋 Cooling ribs
5502 冒口补缩扩展 Riser feed extensions
56 扩展 Extensions 5601 冒口残余 Riser remains
5602 内浇口残余 Ingate remains
5603 出气孔残余 Vent remains
57 冷铁 Chill  5701 冷铁之间的额外金属 Extra metal between chills
5702 冷铁移位造成的多肉 Chill displacement extra
5703 冷铁焊接到铸件上或夹死在铸件上 Welded or clamped chills